Funct. Mater. 2021; 28 1: 39-41.

doi:https://doi.org/10.15407/fm28.01.39

On the high temperature conductivity of ceramics La0.6Sr0.4Co0.2Fe0.8O3-δ -Ce0.8Sm0.2O1.9

Yandong Wang, Lv Ji

Department of Materials Science and Engineering, Jilin Institute of Chemical Technology, 132022 Jilin, China

Abstract: 

Perovskite-type ceramics La0.6Sr0.4Co0.2Fe0.8O3-δ (LSCF) and La0.6Sr0.4Co0.2Fe0.8O3-δ-Ce0.8Sm0.2O1.9(LSCF-GDC) prepared by the method of solid-state reaction were tested by SEM, and their conductivity-temperature relationships were measured by the direct current four-terminal method. The activation energies of small polarons of single-phase LSCF and LSCF-GDC are Ea1 = 9.92 kJ/mol and Ea2 = 12.34 kJ/mol, respectively.

Keywords: 
Perovskite-type ceramics, conductivity-temperature, activation energies.
References: 
1. Alexandros Safakas, Georgios Bampos, Symeon Bebelis, Appl. Catalysis B: Environmental, 244, 225 (2019).
https://doi.org/10.1016/j.apcatb.2018.11.015
 
2. Shadi Darvish, Cheng Cheng Wang, San Ping Jiang, Yu Zhong, Electrochim. Acta, 287, 68 (2018).
https://doi.org/10.1016/j.electacta.2018.04.039
 
3. Valdir Pereira Junior, Priscila Lemes Rachadel, Mara Novy Quadri et al., Ceramics Intern., 44, 20671 (2018).
https://doi.org/10.1016/j.ceramint.2018.08.060
 
4. Sungmee Cho, YoungNam Kim, Jung-Hyun Kim et al., Electrochim, Acta, 56, 5472 (2011).
https://doi.org/10.1016/j.electacta.2011.03.039
 
5. J.D.Castro-Robles, N.Soltani, J.A.Chavez-Carvayar, Mater. Chem. Phys., 225, 50 (2019).
https://doi.org/10.1016/j.matchemphys.2018.12.053
 
6. Kazuyoshi Sato, Chizuru Iwata, Naokatsu Kannari, Hiroya Abe, J. Power Sources, 414, 502 (2019),
https://doi.org/10.1016/j.jpowsour.2019.01.032
 
7. G.S.Kostogloudis, C.Ftikos, Solid State Ionics, 126, 143 (1999).
https://doi.org/10.1016/S0167-2738(99)00230-1
 
8. L.W.Tai, M.M.Nasrallah, H.U.Anderson et al., Solid State Ionics, 76, 273 (1995).
https://doi.org/10.1016/0167-2738(94)00245-N
 

Current number: